RE: Rapid RH probe out of calibration?
It is easy to test isn't it....

One probe in now.
One probe in later.
Compare.

Repeat under different conditions and drying environments.

I will say I just got an IFTI report back and it had 3 equipment malfunctions (no reported %) on it out of 12 tests. aka 25%. I do not believe they use Wagner.