I would ask the manufacturer for their requirements first. If the coating is quite breathable they may be rather lax in their demands.

Typically though almost any finish requires some degree of dryness be inherent in the substrate. You wouldn't put ceramic tile on a 2 day old slab, but 30 days may be fine.

Determining the dryness is rather easy if the slab reaches a temperature conducive for testing. If the concrete never falls below 90 degrees, the rH can read quite low, yet the moisture present could be rather high. Likewise in the winter a cold slab would read artificially low. This is why we test at a standard expected temperature. Outside that range is going to be very wide spread, but you may get a good idea of comparable rH if you can read the slab around 70 degrees.

If the temperature is moving quickly, you may need to insure your probe and the sensor are acclimated also. Can you shade the area you are reading?
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply


Messages In This Thread
RH Testing For Parking Garages - CCR - 07-12-2012, 07:56 AM
RE: RH Testing For Parking Garages - CCR - 07-12-2012, 08:48 AM
RE: RH Testing For Parking Garages - CC Solutions - 07-12-2012, 09:00 AM
RE: RH Testing For Parking Garages - CCR - 07-12-2012, 09:14 AM
RE: RH Testing For Parking Garages - CCR - 07-12-2012, 01:44 PM

Possibly Related Threads...
Thread Author Replies Views Last Post
Wink article on testing eaadams 3 6,300 09-01-2013, 09:10 AM
Last Post: CC Solutions
  No Testing Requirements ???? CCR 3 5,177 06-28-2013, 10:26 AM
Last Post: eaadams
  Moisture Testing Awareness raised Down Under... Horror abounds... Rubensgt40 6 9,608 05-10-2013, 06:46 PM
Last Post: Rubensgt40
  insuti testing jim decker 27 26,869 05-02-2013, 12:31 PM
Last Post: jim decker
  How Do You Charge For Testing? CCR 23 22,576 03-21-2013, 05:05 PM
Last Post: CCR
  RH & CC Testing CCR 23 41,560 07-26-2012, 06:19 AM
Last Post: CC Solutions
  Wood Floor Testing eaadams 1 5,424 06-07-2012, 01:08 PM
Last Post: hnelson

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)