We're almost at 3lbs MVER, so what if the rH is over 90% ?
08-17-2012, 06:01 AM,
#23
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ?
I believe you are right, as the prior version of 2170 did list an 'or' statement.

What we have found is the temperature will affect the readings, so we try to measure the concrete at the service temperature.