We're almost at 3lbs MVER, so what if the rH is over 90% ?
07-12-2012, 01:04 PM,
#2
RE: We're almost at 3lbs MVER, so what if the rH is over 90% ?
Yes there really is a gap in the concrete knowledge on this subject. I used to think the RH Hood method would help alleviate this but it hasn't.

I'd love to see a study on RH Hood tests done next to CaCl to see if there is any parallel.

Hoods are just so expensive... I put those GE probes in mine and they are guaranteed targets for lifts.