RH & CC Testing

#9
I agree, CCR...I wish that all my projects required the testing to be done by an independent, certified agency.

Not only is it beneficial to owners and clients, but to us as contractors as well. I would much rather not be in the position of monitoring the RH of a slab which is waiting for flooring installation, and having the GC question my every move, asserting that my testing MUST be faulty (because the 5" slab that he poured 6 weeks ago is testing in the high 90% and not moving down by leaps and bounds every day **eyeroll**).

Even when you educate them, when they are being ridden by (an unrealistic) schedule, they seem to not get it.

I believe if the testing was done independently, they would have a harder time pressuring us to install the flooring before the concrete is ready.
Erica
Project Manager
Reply


Messages In This Thread
RH & CC Testing - CCR - 07-10-2012, 10:35 AM
RE: RH & CC Testing - CC Solutions - 07-12-2012, 06:37 AM
RE: RH & CC Testing - CCR - 07-12-2012, 07:25 AM
RE: RH & CC Testing - eaadams - 07-12-2012, 01:31 PM
RE: RH & CC Testing - CCR - 07-12-2012, 01:38 PM
RE: RH & CC Testing - CC Solutions - 07-12-2012, 01:48 PM
RE: RH & CC Testing - JLG - 07-17-2012, 11:13 AM
RE: RH & CC Testing - CCR - 07-17-2012, 11:37 AM
RE: RH & CC Testing - Erica - 07-17-2012, 12:10 PM
RE: RH & CC Testing - CCR - 07-17-2012, 12:27 PM
RE: RH & CC Testing - eaadams - 07-18-2012, 11:19 AM
RE: RH & CC Testing - CCR - 07-18-2012, 11:32 AM
RE: RH & CC Testing - CC Solutions - 07-19-2012, 07:49 PM
RE: RH & CC Testing - CCR - 07-22-2012, 04:55 AM
RE: RH & CC Testing - CC Solutions - 07-22-2012, 09:09 AM
RE: RH & CC Testing - CCR - 07-22-2012, 03:05 PM
RE: RH & CC Testing - Rubensgt40 - 07-22-2012, 07:19 PM
RE: RH & CC Testing - CC Solutions - 07-22-2012, 07:33 PM
RE: RH & CC Testing - CCR - 07-24-2012, 04:07 PM
RE: RH & CC Testing - Rubensgt40 - 07-24-2012, 05:35 PM
RE: RH & CC Testing - CC Solutions - 07-24-2012, 05:49 PM
RE: RH & CC Testing - CCR - 07-25-2012, 03:49 AM
RE: RH & CC Testing - Rubensgt40 - 07-25-2012, 09:46 PM
RE: RH & CC Testing - CC Solutions - 07-26-2012, 06:19 AM

Possibly Related Threads...
Thread Author Replies Views Last Post
Wink article on testing eaadams 3 6,270 09-01-2013, 09:10 AM
Last Post: CC Solutions
  No Testing Requirements ???? CCR 3 5,144 06-28-2013, 10:26 AM
Last Post: eaadams
  Moisture Testing Awareness raised Down Under... Horror abounds... Rubensgt40 6 9,551 05-10-2013, 06:46 PM
Last Post: Rubensgt40
  insuti testing jim decker 27 26,746 05-02-2013, 12:31 PM
Last Post: jim decker
  How Do You Charge For Testing? CCR 23 22,505 03-21-2013, 05:05 PM
Last Post: CCR
  RH Testing For Parking Garages CCR 6 9,546 07-12-2012, 01:44 PM
Last Post: CCR
  Wood Floor Testing eaadams 1 5,412 06-07-2012, 01:08 PM
Last Post: hnelson

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)