RH & CC Testing
07-12-2012, 01:48 PM,
#6
RE: RH & CC Testing
I have seen this so often it makes me sick. The ASTM is so simple a 3rd grader could follow it, yet I think about 2% are done correctly.

I believe with the old cut back adhesives and asbestos filled flooring there wasn't the need to find the true MVER and any kind of test will work if the glue can't fail....

Crack tip: I just started using Ardex ArdiFix and it seems to be working well.
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Quote this message in a reply


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious

Messages In This Thread
RH & CC Testing - CCR - 07-10-2012, 10:35 AM
RE: RH & CC Testing - CC Solutions - 07-12-2012, 06:37 AM
RE: RH & CC Testing - CCR - 07-12-2012, 07:25 AM
RE: RH & CC Testing - eaadams - 07-12-2012, 01:31 PM
RE: RH & CC Testing - CCR - 07-12-2012, 01:38 PM
RE: RH & CC Testing - CC Solutions - 07-12-2012, 01:48 PM
RE: RH & CC Testing - JLG - 07-17-2012, 11:13 AM
RE: RH & CC Testing - CCR - 07-17-2012, 11:37 AM
RE: RH & CC Testing - Erica - 07-17-2012, 12:10 PM
RE: RH & CC Testing - CCR - 07-17-2012, 12:27 PM
RE: RH & CC Testing - eaadams - 07-18-2012, 11:19 AM
RE: RH & CC Testing - CCR - 07-18-2012, 11:32 AM
RE: RH & CC Testing - CC Solutions - 07-19-2012, 07:49 PM
RE: RH & CC Testing - CCR - 07-22-2012, 04:55 AM
RE: RH & CC Testing - CC Solutions - 07-22-2012, 09:09 AM
RE: RH & CC Testing - CCR - 07-22-2012, 03:05 PM
RE: RH & CC Testing - Rubensgt40 - 07-22-2012, 07:19 PM
RE: RH & CC Testing - CC Solutions - 07-22-2012, 07:33 PM
RE: RH & CC Testing - CCR - 07-24-2012, 04:07 PM
RE: RH & CC Testing - Rubensgt40 - 07-24-2012, 05:35 PM
RE: RH & CC Testing - CC Solutions - 07-24-2012, 05:49 PM
RE: RH & CC Testing - CCR - 07-25-2012, 03:49 AM
RE: RH & CC Testing - Rubensgt40 - 07-25-2012, 09:46 PM
RE: RH & CC Testing - CC Solutions - 07-26-2012, 06:19 AM