RH & CC Testing

#4
Yea we don't accept CaCl tests anymore. Even people with a P.E. after their name seem to not be able to do it correctly. These pictures done by one of the more respected "professional building testing labs" in California.

Here is an example of this.
[Image: IMG_1475.JPG]




side note: oy the cracks Sad Lumpy Bumpy Slab will probably break poor church's budget. We want to fix the crack with Roadware Concrete Mender but at over $5 lft it is so expensive.

[Image: IMG_1477.JPG]
Reply


Messages In This Thread
RH & CC Testing - CCR - 07-10-2012, 10:35 AM
RE: RH & CC Testing - CC Solutions - 07-12-2012, 06:37 AM
RE: RH & CC Testing - CCR - 07-12-2012, 07:25 AM
RE: RH & CC Testing - eaadams - 07-12-2012, 01:31 PM
RE: RH & CC Testing - CCR - 07-12-2012, 01:38 PM
RE: RH & CC Testing - CC Solutions - 07-12-2012, 01:48 PM
RE: RH & CC Testing - JLG - 07-17-2012, 11:13 AM
RE: RH & CC Testing - CCR - 07-17-2012, 11:37 AM
RE: RH & CC Testing - Erica - 07-17-2012, 12:10 PM
RE: RH & CC Testing - CCR - 07-17-2012, 12:27 PM
RE: RH & CC Testing - eaadams - 07-18-2012, 11:19 AM
RE: RH & CC Testing - CCR - 07-18-2012, 11:32 AM
RE: RH & CC Testing - CC Solutions - 07-19-2012, 07:49 PM
RE: RH & CC Testing - CCR - 07-22-2012, 04:55 AM
RE: RH & CC Testing - CC Solutions - 07-22-2012, 09:09 AM
RE: RH & CC Testing - CCR - 07-22-2012, 03:05 PM
RE: RH & CC Testing - Rubensgt40 - 07-22-2012, 07:19 PM
RE: RH & CC Testing - CC Solutions - 07-22-2012, 07:33 PM
RE: RH & CC Testing - CCR - 07-24-2012, 04:07 PM
RE: RH & CC Testing - Rubensgt40 - 07-24-2012, 05:35 PM
RE: RH & CC Testing - CC Solutions - 07-24-2012, 05:49 PM
RE: RH & CC Testing - CCR - 07-25-2012, 03:49 AM
RE: RH & CC Testing - Rubensgt40 - 07-25-2012, 09:46 PM
RE: RH & CC Testing - CC Solutions - 07-26-2012, 06:19 AM

Possibly Related Threads...
Thread Author Replies Views Last Post
Wink article on testing eaadams 3 6,318 09-01-2013, 09:10 AM
Last Post: CC Solutions
  No Testing Requirements ???? CCR 3 5,192 06-28-2013, 10:26 AM
Last Post: eaadams
  Moisture Testing Awareness raised Down Under... Horror abounds... Rubensgt40 6 9,631 05-10-2013, 06:46 PM
Last Post: Rubensgt40
  insuti testing jim decker 27 27,068 05-02-2013, 12:31 PM
Last Post: jim decker
  How Do You Charge For Testing? CCR 23 22,729 03-21-2013, 05:05 PM
Last Post: CCR
  RH Testing For Parking Garages CCR 6 9,631 07-12-2012, 01:44 PM
Last Post: CCR
  Wood Floor Testing eaadams 1 5,429 06-07-2012, 01:08 PM
Last Post: hnelson

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)