• 3 Vote(s) - 4.33 Average
  • 1
  • 2
  • 3
  • 4
  • 5
Moisture Meters

#1
I have heard that a surface moisture meter is not as good a way to measure moisture in concrete as using an internal relative humidity sensor. Could someone clarify this for me?
Reply


Messages In This Thread
Moisture Meters - concreteworker27 - 09-11-2008, 09:00 AM
RE: Moisture Meters - rthompson - 09-12-2008, 01:28 PM
RE: Moisture Meters - Blake McFee - 09-12-2008, 05:42 PM
RE: Moisture Meters - rthompson - 09-15-2008, 04:19 PM
RE: Moisture Meters - rthompson - 10-21-2008, 11:49 AM

Possibly Related Threads...
Thread Author Replies Views Last Post
  Moisture going up Rubensgt40 3 1,568 07-05-2014, 03:18 AM
Last Post: Rubensgt40
  35-40 year old concrete with moisture problems Tscdad 13 7,385 05-19-2014, 10:55 AM
Last Post: eaadams
  Digital moisture meter QC worker 2 1,871 05-10-2014, 08:07 PM
Last Post: Rubensgt40
  Tandus removes moisture testing requirement eaadams 2 4,100 09-27-2013, 10:26 AM
Last Post: eaadams
  Carbide moisture testing CC Solutions 4 8,688 09-18-2012, 06:11 PM
Last Post: CC Solutions
  Old concrete slab moisture DeanC 23 50,586 12-15-2011, 01:20 AM
Last Post: foxgeorge
  Flooring Manufacturer Warrenty in Relation to Moisture mwoody 5 10,924 08-14-2011, 08:43 PM
Last Post: Ernesto
Sad Is there a way to measure moisture plus cold temperatures sort of like a heat index b Ronald Edberg 4 10,735 07-01-2011, 07:11 PM
Last Post: rthompson
  Concrete Moisture Control Systems BuilderPDX 8 16,850 06-09-2011, 06:09 AM
Last Post: CC Solutions
  The Moisture Webinar Ernesto 17 33,308 04-01-2011, 09:02 PM
Last Post: CC Solutions

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)