You can do a floating subfloor
1 st layer, 3/8" exposure 1 plywood, is not fastened to concrete 1/8" gaping between panels.
2nd layer, 3/8" exposure 1 plywood, is laid perpendicular to first without no edges touching between them.
You then staple the 2nd layer to the 1st layer and proceed to nail to the 3/4" thickness required for nail down installation.
Thus you do not penetrate the vapor retarder.
This is approved by the NWFA and all mfg's in their instructions.
Reply


Messages In This Thread
RE: RH in Concrete for Wood Floor with Vapor Membrane - jim decker - 03-22-2013, 01:36 PM

Possibly Related Threads...
Thread Author Replies Views Last Post
  ICRI pH testing Concrete Repair Bulletin eaadams 4 2,319 05-20-2014, 12:00 PM
Last Post: Ashok Kakade
  35-40 year old concrete with moisture problems Tscdad 13 7,093 05-19-2014, 10:55 AM
Last Post: eaadams
  Concrete Hood Method Blake McFee 9 27,092 11-08-2013, 01:41 PM
Last Post: eaadams
  How thick is your floor? CC Solutions 21 45,011 07-19-2013, 05:14 PM
Last Post: CCR
Question Concrete Cork Sandwich Floor System JKJeremy 4 8,149 01-30-2013, 04:43 PM
Last Post: eaadams
  Vapor Drive / Osmotic Action & RH eaadams 5 12,208 12-15-2012, 06:46 AM
Last Post: CC Solutions
  Self consolidating concrete (SCC) eaadams 32 59,851 05-08-2012, 07:04 AM
Last Post: CC Solutions
  Adhesive/Vapor Retarding Membranes. Ernesto 2 6,609 04-01-2012, 09:08 AM
Last Post: Ernesto
  World of Concrete 2012 eaadams 0 3,406 03-23-2012, 09:40 AM
Last Post: eaadams
  Floor Covering Installer eaadams 2 7,654 12-23-2011, 12:06 PM
Last Post: eaadams

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)