RH in Concrete for Wood Floor with Vapor Membrane

#12
If this is a floating floor and not adhered then first off you should test the slab. If it close to 85% I would do a coat of Bostik MVP4, then a six mil plastic. Then float to your hearts content. Never had a failure with that even below grade using solid hardwood with a floating ply subfloor.

Heck even the new Bostik Single App says it will warranty a slab below 85% with no barrier under the slab.
Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Reply


Messages In This Thread
RE: RH in Concrete for Wood Floor with Vapor Membrane - Ernesto - 06-20-2012, 08:00 PM

Possibly Related Threads...
Thread Author Replies Views Last Post
  ICRI pH testing Concrete Repair Bulletin eaadams 4 2,403 05-20-2014, 12:00 PM
Last Post: Ashok Kakade
  35-40 year old concrete with moisture problems Tscdad 13 7,331 05-19-2014, 10:55 AM
Last Post: eaadams
  Concrete Hood Method Blake McFee 9 27,266 11-08-2013, 01:41 PM
Last Post: eaadams
  How thick is your floor? CC Solutions 21 45,383 07-19-2013, 05:14 PM
Last Post: CCR
Question Concrete Cork Sandwich Floor System JKJeremy 4 8,218 01-30-2013, 04:43 PM
Last Post: eaadams
  Vapor Drive / Osmotic Action & RH eaadams 5 12,267 12-15-2012, 06:46 AM
Last Post: CC Solutions
  Self consolidating concrete (SCC) eaadams 32 60,337 05-08-2012, 07:04 AM
Last Post: CC Solutions
  Adhesive/Vapor Retarding Membranes. Ernesto 2 6,655 04-01-2012, 09:08 AM
Last Post: Ernesto
  World of Concrete 2012 eaadams 0 3,427 03-23-2012, 09:40 AM
Last Post: eaadams
  Floor Covering Installer eaadams 2 7,712 12-23-2011, 12:06 PM
Last Post: eaadams

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)