I attended a wood flooring job where a slab took moisture from a plumbing failure. There was poly sheeting on the slab, 12mm ply then 13mm overlay solid timber. The whole thing buckled like buggery. So there are definitely points which poly cannot withstand. As JD always advises- see what the warranty says!
The problem with socialism is that you soon run out of other people's money.
- Margaret Thatcher

Reply


Messages In This Thread
RE: RH in Concrete for Wood Floor with Vapor Membrane - Rubensgt40 - 06-18-2012, 04:55 PM

Possibly Related Threads...
Thread Author Replies Views Last Post
  ICRI pH testing Concrete Repair Bulletin eaadams 4 2,389 05-20-2014, 12:00 PM
Last Post: Ashok Kakade
  35-40 year old concrete with moisture problems Tscdad 13 7,270 05-19-2014, 10:55 AM
Last Post: eaadams
  Concrete Hood Method Blake McFee 9 27,234 11-08-2013, 01:41 PM
Last Post: eaadams
  How thick is your floor? CC Solutions 21 45,317 07-19-2013, 05:14 PM
Last Post: CCR
Question Concrete Cork Sandwich Floor System JKJeremy 4 8,203 01-30-2013, 04:43 PM
Last Post: eaadams
  Vapor Drive / Osmotic Action & RH eaadams 5 12,237 12-15-2012, 06:46 AM
Last Post: CC Solutions
  Self consolidating concrete (SCC) eaadams 32 60,145 05-08-2012, 07:04 AM
Last Post: CC Solutions
  Adhesive/Vapor Retarding Membranes. Ernesto 2 6,641 04-01-2012, 09:08 AM
Last Post: Ernesto
  World of Concrete 2012 eaadams 0 3,424 03-23-2012, 09:40 AM
Last Post: eaadams
  Floor Covering Installer eaadams 2 7,692 12-23-2011, 12:06 PM
Last Post: eaadams

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)