RH test results varying
05-08-2012, 06:49 PM,
#6
RE: RH test results varying
(warning: posting without prior research...Smile)

Isn't there a bit in F2170, besides the bit about service temperature, which says the probe and the concrete must be the same temperature at the time of the reading?

Which means you need to use one of those point-and-shoot infrared thermometers to check both before taking the reading...
The problem with socialism is that you soon run out of other people's money.
- Margaret Thatcher

Quote this message in a reply


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious

Messages In This Thread
RH test results varying - Erica - 04-30-2012, 02:20 PM
RE: RH test results varying - rapidrhrep - 05-01-2012, 08:13 AM
RE: RH test results varying - Erica - 05-01-2012, 08:27 AM
RE: RH test results varying - eaadams - 05-07-2012, 09:43 AM
RE: RH test results varying - CC Solutions - 05-07-2012, 01:07 PM
RE: RH test results varying - Rubensgt40 - 05-08-2012, 06:49 PM
RE: RH test results varying - CC Solutions - 05-09-2012, 06:05 AM
RE: RH test results varying - Rubensgt40 - 05-09-2012, 04:35 PM