Ardex V1200

#19
I had the opportunity to test a self-leveler very similar to V1200 from a newer manufacturer recently. While it was "OK", it didn't spread and finish like Ardex...simple as that. Ya get what ya pay for every time no matter what.
JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com
Reply


Messages In This Thread
Ardex V1200 - CC Solutions - 03-27-2012, 09:57 AM
RE: Ardex V1200 - eaadams - 03-27-2012, 10:03 AM
RE: Ardex V1200 - CC Solutions - 03-27-2012, 10:36 AM
RE: Ardex V1200 - eaadams - 04-25-2012, 02:01 PM
RE: Ardex V1200 - CC Solutions - 04-25-2012, 04:06 PM
RE: Ardex V1200 - CCR - 04-26-2012, 04:36 AM
RE: Ardex V1200 - CC Solutions - 04-26-2012, 06:11 AM
RE: Ardex V1200 - CCR - 04-26-2012, 07:11 AM
RE: Ardex V1200 - CC Solutions - 04-26-2012, 07:18 AM
RE: Ardex V1200 - CCR - 04-26-2012, 07:33 AM
RE: Ardex V1200 - CC Solutions - 04-26-2012, 07:16 PM
RE: Ardex V1200 - eaadams - 04-26-2012, 08:36 PM
RE: Ardex V1200 - CC Solutions - 04-27-2012, 06:06 AM
RE: Ardex V1200 - eaadams - 05-07-2012, 09:45 AM
RE: Ardex V1200 - CC Solutions - 05-07-2012, 12:27 PM
RE: Ardex V1200 - eaadams - 07-10-2012, 10:28 AM
RE: Ardex V1200 - CCR - 07-10-2012, 11:40 AM
RE: Ardex V1200 - CC Solutions - 07-12-2012, 06:19 AM
RE: Ardex V1200 - CCR - 07-12-2012, 07:49 AM
RE: Ardex V1200 - CC Solutions - 07-12-2012, 08:10 AM
RE: Ardex V1200 - eaadams - 07-12-2012, 12:56 PM
RE: Ardex V1200 - CC Solutions - 07-12-2012, 01:33 PM
RE: Ardex V1200 - eaadams - 07-12-2012, 01:42 PM
RE: Ardex V1200 - CC Solutions - 07-12-2012, 01:50 PM
RE: Ardex V1200 - CCR - 07-12-2012, 02:46 PM
RE: Ardex V1200 - CC Solutions - 07-12-2012, 04:25 PM

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)