99 % RH

#2
Unless they're willing to sign a waiver releasing you from moisture related flooring failures, I wouldn't touch this one...not at 18,000 sf. Too many businesses that operate 365 days a year "just don't get it" when it comes to fixing moisture related issues. Honestly, it's like ignoring the doctor when he says you have cancer.