Rrozema:

1) Having a copy of the ASTM F2170 standard for which the Rapid RH was designed to meet, is a must. Have you ever been given one? I find the answer to this to be no more times than not when I talk to people. This should not be on you.

2) I have a hard time believing that the pour on this pan is this shallow. Usually the shallow part would be around this deep but not the deep section of the pan. With that being said, alot of people will cut the top of the barrel off on shallow pours such as gypsum where it is being used for soundproofing.

3) Determining whether 20% or 40%-Is the slab drying from one or two sides? Any pan decking on the market, even "vented" decking, is only drying from one side, thus 40% is required. The easiest way to determine whether the slab is open on the bottom is go to the lower level and look up. Can you see concrete or corrugated metal?

Hope this helps!

Jason
Reply


Messages In This Thread
improper probe depth - Rrozema - 02-23-2012, 01:00 PM
RE: improper probe depth - rapidrhrep - 02-23-2012, 01:51 PM
RE: improper probe depth - Rrozema - 02-23-2012, 02:22 PM
RE: improper probe depth - Rrozema - 02-28-2012, 08:44 AM
RE: improper probe depth - rapidrhrep - 03-01-2012, 07:43 AM
RE: improper probe depth - CC Solutions - 03-01-2012, 12:47 PM
RE: improper probe depth - Rubensgt40 - 03-04-2012, 03:56 PM
RE: improper probe depth - CCR - 03-09-2012, 06:14 AM
RE: improper probe depth - GP-CA - 03-23-2012, 02:24 PM
RE: improper probe depth - Ernesto - 03-23-2012, 07:51 PM
RE: improper probe depth - CC Solutions - 03-24-2012, 06:12 AM

Possibly Related Threads...
Thread Author Replies Views Last Post
  Ardex promotes the Wagner Rapid RH probe! CC Solutions 15 35,057 01-15-2012, 06:33 PM
Last Post: CC Solutions
  Relative Humidity Probe Depth mwoody 10 22,655 03-24-2011, 07:00 AM
Last Post: CC Solutions
  Probe Placement (Depth) CDougherty 2 8,892 01-15-2010, 09:43 PM
Last Post: CC Solutions
  Hole Depth Jphillips 1 7,505 02-20-2009, 12:54 PM
Last Post: rthompson

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
2 Guest(s)