MMS- Are some unreliable with high RH?

#9
And of course the permeability of concrete can vary, but I have read that 4" of concrete has a perm rate of less than .8...

The numbers quoted for perm ratings are all over the place aren't they? Makes it hard to compare. I believe Bostik reports grams of water over 24 hrs over a square meter, and then that is at 50% RH. What does that mean? 50% difference between slab and ambient?

Koster VAP1-2000FS which I use is an average of .05 grains /hr/sf. A gram is about 15 grains....
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply


Messages In This Thread
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-07-2011, 04:16 PM

Possibly Related Threads...
Thread Author Replies Views Last Post
  Who Says Rapid Rh Reads High? Ernesto 3 9,348 08-20-2012, 07:07 PM
Last Post: CC Solutions
  High Rapid RH readings?? ddemento 49 81,512 12-08-2011, 06:03 PM
Last Post: Ernesto
  high rh in concrete chas04344 2 8,942 09-11-2009, 07:33 PM
Last Post: chas04344

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)