MMS- Are some unreliable with high RH?

#8
To give you an idea:
ASTM E96 Bostic Moisture Seal's Perm Rating is: 0.12 g/24 hrs/M²mmHg @ 32° C and 50% RH
source: http://bostik.com.au/construction-trade-products-catalogue-sheet-28565-moisture_seal-m-0-g-0.html

ASTM E96 - Koster VAP perm Rating is: 0.024 grams h-1 m-2
source: http://www.kosterusa.com/files/us_en/6.035-VAP-2000.pdf

And as a benchmark:
ASTM E 1745 - Stego wrap has perm: 0.0084 (but I can't find metric #'s for it)

http://www.stegoindustries.com/faqs/what_is_the_difference_between_a_vapor_barrier_and_a_vapor_retarder.html
**Section 7 of ASTM E 1745 specifies the testing conditions and allows for either of the following test methods: ASTM F1249 or ASTM E96.

Reply


Messages In This Thread
RE: MMS- Are some unreliable with high RH? - eaadams - 11-07-2011, 03:22 PM

Possibly Related Threads...
Thread Author Replies Views Last Post
  Who Says Rapid Rh Reads High? Ernesto 3 9,306 08-20-2012, 07:07 PM
Last Post: CC Solutions
  High Rapid RH readings?? ddemento 49 81,072 12-08-2011, 06:03 PM
Last Post: Ernesto
  high rh in concrete chas04344 2 8,906 09-11-2009, 07:33 PM
Last Post: chas04344

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)