MMS- Are some unreliable with high RH?

#5
Great question Pat, it is one that confuses me also.

The specs and requirements of MMS manufacturers I am familiar with all vary somewhat. Some will not warrant their product unless there is a vapor retarder under the slab. Some limit RH to 95% or less. One is limited to 98% RH. Many warrant to any RH, but will deny coverage because the alkalinity is too high.

Why am I confused when these numbers seem so clearly defined? The numbers are not firm. The MMS I mentioned that is good to 95% RH is a two part 100% solid epoxy system. I mentioned to my factory rep that I had a project with no vapor retarder and a history of failure. These are the worst possible parameters and RH values can reach 99%. No worries I was told, the technical team has approved the use of our MMS on that slab. Huh
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply


Messages In This Thread
RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-07-2011, 07:23 AM

Possibly Related Threads...
Thread Author Replies Views Last Post
  Who Says Rapid Rh Reads High? Ernesto 3 9,313 08-20-2012, 07:07 PM
Last Post: CC Solutions
  High Rapid RH readings?? ddemento 49 81,125 12-08-2011, 06:03 PM
Last Post: Ernesto
  high rh in concrete chas04344 2 8,914 09-11-2009, 07:33 PM
Last Post: chas04344

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)