Thanks Evan. I suppose I'm trying to build the alibi for regular testing regimen- too many contractors still say "Don't worry, we're just gonna slap down a vapour barrier".

The manufacturer in question (I won't name them, and I don't expect anyone on this thread to name anyone in these types of discussions!) fully believed from their R & D that their product was a one coat system. The fact that they responded to a failure by tightening their specs, when it means they will possibly sell less product, not to mention wore a lot of cost, is one of the reasons we will continue to deal with them.

Some guys put down plastic sheeting, then plywood, then overlay timber flooring. Is this a reliable mitigation against slab moisture?

The problem with socialism is that you soon run out of other people's money.
- Margaret Thatcher

Reply


Messages In This Thread
RE: MMS- Are some unreliable with high RH? - Rubensgt40 - 11-06-2011, 06:19 PM

Possibly Related Threads...
Thread Author Replies Views Last Post
  Who Says Rapid Rh Reads High? Ernesto 3 9,303 08-20-2012, 07:07 PM
Last Post: CC Solutions
  High Rapid RH readings?? ddemento 49 81,032 12-08-2011, 06:03 PM
Last Post: Ernesto
  high rh in concrete chas04344 2 8,897 09-11-2009, 07:33 PM
Last Post: chas04344

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)