Bottom line, you have a wet slab.

RH levels do actually fall rather quickly once the slab starts drying. By rather quickly I mean a 1 - 2 points a week if conditions are right.

As long as you have done the testing according to the instructions in your test kit, you can trust the readings. You should be 2.4" into the slab, brushed and vacuumed holes, drilled straight and true, you don't wet drill right?

If it makes you feel any better, I did a job last fall where they waited 16 months for suspended floors to dry and they were still at 98%. The 4" slab on grade areas were down to the mid 80's to low 90's.
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply


Messages In This Thread
High Rapid RH readings?? - ddemento - 11-03-2011, 12:13 PM
RE: High Rapid RH readings?? - eaadams - 11-03-2011, 12:33 PM
RE: High Rapid RH readings?? - ddemento - 11-07-2011, 12:58 PM
RE: High Rapid RH readings?? - eaadams - 11-07-2011, 01:20 PM
RE: High Rapid RH readings?? - eaadams - 11-07-2011, 01:52 PM
RE: High Rapid RH readings?? - Ernesto - 11-07-2011, 07:27 PM
RE: High Rapid RH readings?? - eaadams - 11-07-2011, 08:33 PM
RE: High Rapid RH readings?? - eaadams - 11-08-2011, 09:38 AM
RE: High Rapid RH readings?? - eaadams - 11-08-2011, 10:11 AM
RE: High Rapid RH readings?? - ddemento - 11-09-2011, 05:00 AM
RE: High Rapid RH readings?? - eaadams - 11-09-2011, 08:20 PM
RE: High Rapid RH readings?? - ddemento - 11-11-2011, 11:07 AM
RE: High Rapid RH readings?? - CC Solutions - 11-11-2011, 11:18 AM
RE: High Rapid RH readings?? - eaadams - 11-11-2011, 11:23 AM
RE: High Rapid RH readings?? - Ernesto - 11-11-2011, 04:36 PM
RE: High Rapid RH readings?? - eaadams - 11-11-2011, 08:49 PM
RE: High Rapid RH readings?? - Ernesto - 11-12-2011, 05:07 PM
RE: High Rapid RH readings?? - Ernesto - 11-12-2011, 05:45 PM
RE: High Rapid RH readings?? - ddemento - 11-16-2011, 10:05 AM
RE: High Rapid RH readings?? - eaadams - 11-16-2011, 10:50 AM
RE: High Rapid RH readings?? - eaadams - 11-16-2011, 11:32 AM
RE: High Rapid RH readings?? - ddemento - 11-16-2011, 01:25 PM
RE: High Rapid RH readings?? - Rubensgt40 - 11-16-2011, 03:34 PM
RE: High Rapid RH readings?? - eaadams - 11-16-2011, 04:28 PM
RE: High Rapid RH readings?? - Ernesto - 11-16-2011, 05:03 PM
RE: High Rapid RH readings?? - eaadams - 11-16-2011, 06:21 PM
RE: High Rapid RH readings?? - Ernesto - 11-16-2011, 06:43 PM
RE: High Rapid RH readings?? - ddemento - 11-17-2011, 06:16 AM
RE: High Rapid RH readings?? - eaadams - 11-17-2011, 10:13 AM
RE: High Rapid RH readings?? - Ernesto - 11-17-2011, 04:58 PM
RE: High Rapid RH readings?? - ddemento - 12-08-2011, 12:03 PM
RE: High Rapid RH readings?? - Ernesto - 12-08-2011, 12:48 PM
RE: High Rapid RH readings?? - eaadams - 12-08-2011, 05:55 PM
RE: High Rapid RH readings?? - Ernesto - 12-08-2011, 06:03 PM

Possibly Related Threads...
Thread Author Replies Views Last Post
  Who Says Rapid Rh Reads High? Ernesto 3 9,342 08-20-2012, 07:07 PM
Last Post: CC Solutions
  Ardex promotes the Wagner Rapid RH probe! CC Solutions 15 35,203 01-15-2012, 06:33 PM
Last Post: CC Solutions
  MMS- Are some unreliable with high RH? Rubensgt40 64 102,269 11-17-2011, 07:56 AM
Last Post: CC Solutions
  No Love - August Rapid RH Newsletter eaadams 4 9,377 08-19-2011, 07:13 AM
Last Post: CC Solutions
  A GC wants a second opinion, and the first readings were Wagner's! CC Solutions 2 6,826 08-14-2011, 07:56 PM
Last Post: Ernesto
  Multiple Readings? GregR 6 13,729 11-19-2010, 05:26 PM
Last Post: CC Solutions
  high rh in concrete chas04344 2 8,936 09-11-2009, 07:33 PM
Last Post: chas04344
  Rh readings dennismck 1 7,947 10-15-2008, 11:00 AM
Last Post: rthompson

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)