I've done a little homework since asking this question so I'll share with you some of what I found so far (I didn't find a lot out there on this). Personally, I doubt I will ever use the hood method. The only difference I see between it and the calcium chloride test is that it's measuring RH instead of MVER. It's still only measuring at the surface. I was reading an article in FCI that backed up what Trever said, that the readings run lower than the in-situ probes. Why would I want to risk my butt on something that is going to tell me I'm ok when I'm not?! I'm still interested in hearing if anyone has had good/bad experiences, but from what I've read so far, the convenience of not drilling does not unreliable readings.
Here are a couple of links to some of the stuff I found about ASTM F2420:
http://www.fcimag.com/Articles/Feature_Article/8785b318a1cac010VgnVCM100000f932a8c0
http://www.youtube.com/watch?v=51Mbobdcffs
Quote this message in a reply


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious

Messages In This Thread
Concrete Hood Method - Blake McFee - 03-25-2009, 09:18 AM
RE: Concrete Hood Method - rthompson - 04-24-2009, 09:49 AM
RE: Concrete Hood Method - Trever Shiplee - 04-29-2009, 11:27 PM
RE: Concrete Hood Method - WeldKaye - 10-21-2009, 09:41 PM
RE: Concrete Hood Method - Blake McFee - 10-23-2009, 10:02 AM
RE: Concrete Hood Method - CC Solutions - 12-16-2009, 11:39 AM
RE: Concrete Hood Method - CC Solutions - 12-17-2009, 09:33 AM
RE: Concrete Hood Method - eaadams - 11-08-2013, 01:41 PM