Thread Rating:
  • 0 Vote(s) - 0 Average
  • 1
  • 2
  • 3
  • 4
  • 5
Wagner @ WOC 2012
10-22-2011, 05:41 AM,
#14
RE: Wagner @ WOC 2012
I am familiar with the test. The slab was sealed! That was the whole point of the study wasn't it? It showed how mechanically sealing the concrete can retain moisture.
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Quote this message in a reply


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious

Messages In This Thread
Wagner @ WOC 2012 - eaadams - 10-18-2011, 10:05 PM
RE: Wagner @ WOC 2012 - EWagner - 10-19-2011, 10:43 AM
RE: Wagner @ WOC 2012 - eaadams - 10-19-2011, 11:14 AM
RE: Wagner @ WOC 2012 - CC Solutions - 10-19-2011, 01:13 PM
RE: Wagner @ WOC 2012 - EWagner - 10-21-2011, 11:36 AM
RE: Wagner @ WOC 2012 - eaadams - 10-21-2011, 11:50 AM
RE: Wagner @ WOC 2012 - CC Solutions - 10-21-2011, 12:27 PM
RE: Wagner @ WOC 2012 - rapidrhrep - 10-21-2011, 01:04 PM
RE: Wagner @ WOC 2012 - Ernesto - 10-21-2011, 06:08 PM
RE: Wagner @ WOC 2012 - eaadams - 10-21-2011, 06:15 PM
RE: Wagner @ WOC 2012 - Ernesto - 10-21-2011, 07:26 PM
RE: Wagner @ WOC 2012 - CC Solutions - 10-21-2011, 07:33 PM
RE: Wagner @ WOC 2012 - eaadams - 10-21-2011, 08:46 PM
RE: Wagner @ WOC 2012 - CC Solutions - 10-22-2011, 05:41 AM