04-24-2009, 09:44 AM,
#2
RE: How much is too much?
uvpete
I am not sure what the CM% is. I think it is Concrete Moisture percentage by volume. Wet concrete is about 9% by volume. So a 2 - 5% reading would make sense. The problem with this type of measurment is that concrete density and metal in the concrete can give false negatives.