Hi all. First time on the thread. I'm involved in the timber flooring industry down here in Australia (pronounced: Oz-stray-ya), where our standards are yet to catch up to the US. Subsequently, RH moisture testing is a very under-utilized practice at the moment. I look forward to joining the discussions here.

Question, and apologies if it has been asked a million times: I note the instructional video on temperatures having little effect on the RH of the slab. What about the ambient humidity of the area?

A major adhesives manufacturer rep mentioned to me that the highest number of moisture-related flooring failures occurred in a state which is known for its hot, dry climate. This is particularly telling as this area is a much smaller market than the eastern states, with areas known for their higher humidity.

Pardon my ignorance, does this imply that the inherent slab moisture (roughly the same in all locations, give or take differing mixing techniques between concrete layers) will translate to greater RH at the floor covering area, when exposed to a drier hot climate, as opposed to a more humid environment?

Or should it mean that the RH of the slab in a drier, hotter area will decrease more quickly?

Cheers
Pat of Oz
The problem with socialism is that you soon run out of other people's money.
- Margaret Thatcher

Reply


Messages In This Thread
Ambient humidity vs. RH - Rubensgt40 - 10-04-2011, 09:29 PM
RE: Ambient humidity vs. RH - CC Solutions - 10-06-2011, 06:41 AM
RE: Ambient humidity vs. RH - Ernesto - 10-06-2011, 03:43 PM
RE: Ambient humidity vs. RH - Rubensgt40 - 10-06-2011, 05:16 PM
RE: Ambient humidity vs. RH - CC Solutions - 10-06-2011, 06:43 PM
RE: Ambient humidity vs. RH - Rubensgt40 - 10-06-2011, 09:20 PM
RE: Ambient humidity vs. RH - CC Solutions - 10-07-2011, 06:07 AM
RE: Ambient humidity vs. RH - Rubensgt40 - 10-08-2011, 12:24 AM
RE: Ambient humidity vs. RH - Ernesto - 10-08-2011, 01:42 PM
RE: Ambient humidity vs. RH - Rubensgt40 - 10-09-2011, 12:58 AM
RE: Ambient humidity vs. RH - eblakewi - 10-10-2011, 11:21 AM
RE: Ambient humidity vs. RH - CC Solutions - 10-10-2011, 11:37 AM
RE: Ambient humidity vs. RH - Rubensgt40 - 10-10-2011, 02:53 PM
RE: Ambient humidity vs. RH - CC Solutions - 10-10-2011, 03:47 PM
RE: Ambient humidity vs. RH - Rubensgt40 - 10-11-2011, 04:32 PM
RE: Ambient humidity vs. RH - CC Solutions - 10-12-2011, 06:15 AM
RE: Ambient humidity vs. RH - Rubensgt40 - 10-13-2011, 09:12 PM
RE: Ambient humidity vs. RH - CC Solutions - 10-14-2011, 06:12 AM
RE: Ambient humidity vs. RH - Rubensgt40 - 10-16-2011, 02:42 PM
RE: Ambient humidity vs. RH - CC Solutions - 10-16-2011, 06:09 PM

Possibly Related Threads...
Thread Author Replies Views Last Post
  Relative Humidity Probes Blake McFee 5 12,580 08-28-2011, 02:02 PM
Last Post: CC Solutions
  Relative Humidity Probe Depth mwoody 10 22,763 03-24-2011, 07:00 AM
Last Post: CC Solutions
  Specific humidity or ERH or Calcium Carbide? Andy 11 25,722 05-11-2010, 03:22 PM
Last Post: CC Solutions
  Recalibration of Relative Humidity Probes jpeters 7 18,944 12-17-2009, 12:16 PM
Last Post: CC Solutions
  Relative Humidity Probes CMoore 1 7,870 02-20-2009, 01:08 PM
Last Post: rthompson

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)