Hole Depth

#1
I know the requirement is 40% of slab thickness.
We are getting some very high RH readings (20% higher than the tramex readings) using these probes.
Would RH readings increase as the volume of the space beneath the reader increases?
I am not sure if the technician seated the probes properly (all the way on the bottom of the hole) and if he didn't, can i just push them all the way down and receive accurate readings?
Thanks
Reply


Messages In This Thread
Hole Depth - Jphillips - 02-06-2009, 10:44 AM
RE: Hole Depth - rthompson - 02-20-2009, 12:54 PM

Possibly Related Threads...
Thread Author Replies Views Last Post
  improper probe depth Rrozema 10 23,968 03-24-2012, 06:12 AM
Last Post: CC Solutions
  Relative Humidity Probe Depth mwoody 10 22,582 03-24-2011, 07:00 AM
Last Post: CC Solutions
  Probe Placement (Depth) CDougherty 2 8,868 01-15-2010, 09:43 PM
Last Post: CC Solutions
  creating the hole for the sensor SDJeff 1 6,877 11-09-2009, 04:39 PM
Last Post: Ben
  RH Test Hole Callout Ben 3 11,247 11-04-2008, 10:03 AM
Last Post: rthompson

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)