@EA-2170-11 changes in a nutshell (and its better to read yourself in case I miss something):

1) Dictates specifically how far, from the bottom of the hole, the sensor can "live". .625 +- .125
2) Dictates that sensor sleeves must line hole completely from top to bottom.
3) Sleeve must have ribs/fins at bottom of sleeve and at the .625 of the sleeve. This is to isolate the sleeve from the concrete. Must also have an isolation gasket inside the sleeve at the .625 from bottom depth to isolate the sensor from the sleeve. Bottomline, they are trying to do what they can to isolate that very small space of air at .625" from bottom of hole. SOUND FAMILIAR?
4) Sensor must only obtain readings from the bottom of the sleeve. No knockouts and reading from the side.

You should get the standard, there are pictures that do better at explaining.

@JD-"post the ASTM for review"-NICE!! If I had your money I would burn mine. Big Grin An ATV with power steering--Must be nice!

Jason
Reply


Messages In This Thread
ASTM 2170-11 - eaadams - 09-30-2011, 04:00 PM
RE: ASTM 2170-11 - CC Solutions - 10-01-2011, 05:35 AM
RE: ASTM 2170-11 - eaadams - 10-01-2011, 08:36 AM
RE: ASTM 2170-11 - CC Solutions - 10-03-2011, 07:05 AM
RE: ASTM 2170-11 - rapidrhrep - 10-03-2011, 08:23 AM
RE: ASTM 2170-11 - CC Solutions - 10-03-2011, 08:36 AM
RE: ASTM 2170-11 - Ernesto - 10-03-2011, 01:10 PM
RE: ASTM 2170-11 - CC Solutions - 10-03-2011, 01:16 PM
RE: ASTM 2170-11 - eaadams - 10-03-2011, 01:27 PM
RE: ASTM 2170-11 - Ernesto - 10-03-2011, 02:15 PM
RE: ASTM 2170-11 - CC Solutions - 10-03-2011, 02:21 PM
RE: ASTM 2170-11 - Ernesto - 10-03-2011, 02:23 PM
RE: ASTM 2170-11 - rapidrhrep - 10-03-2011, 03:30 PM
RE: ASTM 2170-11 - CC Solutions - 10-03-2011, 04:10 PM
RE: ASTM 2170-11 - eaadams - 10-12-2011, 04:31 PM
RE: ASTM 2170-11 - rapidrhrep - 10-12-2011, 04:54 PM
RE: ASTM 2170-11 - CC Solutions - 10-12-2011, 07:00 PM
RE: ASTM 2170-11 - Ernesto - 10-13-2011, 06:50 AM
RE: ASTM 2170-11 - CC Solutions - 10-13-2011, 07:06 AM
RE: ASTM 2170-11 - Ernesto - 10-13-2011, 02:59 PM
RE: ASTM 2170-11 - Rubensgt40 - 10-16-2011, 03:47 PM
RE: ASTM 2170-11 - CC Solutions - 10-16-2011, 05:53 PM
RE: ASTM 2170-11 - Rubensgt40 - 10-16-2011, 11:13 PM
RE: ASTM 2170-11 - CC Solutions - 10-17-2011, 06:00 AM
RE: ASTM 2170-11 - rapidrhrep - 10-17-2011, 08:38 AM
RE: ASTM 2170-11 - CC Solutions - 10-17-2011, 08:49 AM
RE: ASTM 2170-11 - eaadams - 10-25-2011, 09:04 PM
RE: ASTM 2170-11 - Rubensgt40 - 10-31-2011, 05:30 AM
RE: ASTM 2170-11 - eaadams - 10-31-2011, 11:17 AM
RE: ASTM 2170-11 - CC Solutions - 10-31-2011, 11:31 AM
RE: ASTM 2170-11 - rapidrhrep - 10-31-2011, 12:41 PM
RE: ASTM 2170-11 - CC Solutions - 10-31-2011, 01:57 PM
RE: ASTM 2170-11 - eaadams - 10-31-2011, 11:36 PM

Possibly Related Threads...
Thread Author Replies Views Last Post
  ASTM 2170-11 eaadams 0 818 04-15-2014, 09:33 AM
Last Post: eaadams
  ASTM F3010 - 13 eaadams 1 2,794 02-25-2014, 05:54 PM
Last Post: CC Solutions

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)