Successful floor repair after failure!
09-27-2011, 06:33 AM,
#4
RE: Successful floor repair after failure!
(09-26-2011, 06:16 PM)CC Solutions Wrote:  Yes, they are used all the time, especially to remove asbestos enriched adhesive. Confused

I've inspected a couple of floors where stripper...the orange oil stuff was used to remove cutbac adhesives then a wood floor glued to the slab. Turned into a floater real quick! On one of them the enduser contracted out the company because the box store told them it needed to be removed prior to installation and they would not do it.

The box store got away with it because they didn't put the stripper on.Dodgy I thought they should have done a bond test first but we all know they never do that kinda stuff.

Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Quote this message in a reply


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious

Messages In This Thread
RE: Successful floor repair after failure! - Ernesto - 09-27-2011, 06:33 AM