Self consolidating concrete (SCC)

#24
I had a slab I worked on that was poured with a very high ratio, I'd have to get the old papers out to see how high it was, but it was wet, like .65 or more.

It dried really quickly, much faster than any of us figured it would. Then we thought perhaps it was all the voids that helped it dry. There may be something to that, but the concrete was pretty weak. Good enough for a floor slab though.
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply


Messages In This Thread
RE: Self consolidating concrete (SCC) - CC Solutions - 10-03-2011, 08:32 AM

Possibly Related Threads...
Thread Author Replies Views Last Post
  ICRI pH testing Concrete Repair Bulletin eaadams 4 2,401 05-20-2014, 12:00 PM
Last Post: Ashok Kakade
  35-40 year old concrete with moisture problems Tscdad 13 7,321 05-19-2014, 10:55 AM
Last Post: eaadams
  Concrete Hood Method Blake McFee 9 27,263 11-08-2013, 01:41 PM
Last Post: eaadams
  RH in Concrete for Wood Floor with Vapor Membrane eaadams 35 63,875 05-01-2013, 07:20 AM
Last Post: jim decker
Question Concrete Cork Sandwich Floor System JKJeremy 4 8,218 01-30-2013, 04:43 PM
Last Post: eaadams
  World of Concrete 2012 eaadams 0 3,427 03-23-2012, 09:40 AM
Last Post: eaadams
  Old concrete slab moisture DeanC 23 50,536 12-15-2011, 01:20 AM
Last Post: foxgeorge
  Self-leveling concrete - My bonehead mistake CC Solutions 37 65,550 09-20-2011, 10:07 AM
Last Post: CC Solutions
  Concrete Surface Texture eaadams 12 26,966 06-21-2011, 11:47 AM
Last Post: CC Solutions
  Concrete Moisture Control Systems BuilderPDX 8 16,831 06-09-2011, 06:09 AM
Last Post: CC Solutions

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)