Ceramic Tile & Moisture Testing
02-20-2009, 01:00 PM,
#2
RE: Ceramic Tile & Moisture Testing
(01-30-2009, 09:18 AM)moonrock1 Wrote:  I have been installing ceramic tile over 30 years & we have never been ask to moisture test concrete,untill now. Why the sudden change about the effects that moisture has on ceramic tile when we use a cement base material to in stall our product? The most series problems we have to deal with is expansion & Contraction joints,an if installed correctly,there is very few problems with that.

Thanks Joe

Joe,
You are quite correct. The reason is there are more problems wiith efflorence and sub-efflorence which is a by product of moisture.
Respectfully
Rayt