Scissor Lift knocing off probe tops.

#2
Dirt can be vacuumed or blown out of the sensor tube, usually with no problem.

Placing a cone over the test site is like placing a bullseye on something. They will hit it for sure!!! But seriously, anything that will disrupt or impede the drying of the slab will affect the RH in that area. So I would say placing a sealed 16" diameter rubber cone over the test site will hold vapor emissions and slow the slab's drying in that area. A small open top cone may effect drying a slight bit, but probably not enough to cause a noticeable difference.

I always try to put tests in locations that people aren't driving over the caps.
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply


Messages In This Thread
RE: Scissor Lift knocing off probe tops. - CC Solutions - 08-31-2011, 02:59 PM

Possibly Related Threads...
Thread Author Replies Views Last Post
  Can tape over the probe cause erroneous readings? CC Solutions 22 38,347 06-03-2014, 03:49 PM
Last Post: Ernesto

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)