Thread Rating:
  • 0 Vote(s) - 0 Average
  • 1
  • 2
  • 3
  • 4
  • 5
City Supervisors Meeting
09-04-2011, 10:41 AM,
#13
RE: City Supervisors Meeting
(09-04-2011, 09:22 AM)Ernesto Wrote:  
(09-04-2011, 06:36 AM)CC Solutions Wrote:  You got me there. If you are putting wood floors on bad slabs then yes moisture can be the issue.

Why do you use these trowel on vapor retarders? Especially if you keep having failures using them! What do you tell your clients when these failures happen?

Who said I have had these problems? Are you talkin to me? Big GrinTongue

Uhhh, yeah! Tongue I don't have any buckling wood floors, but I've never used a trowel on vapor retarder either.... Big Grin
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Quote this message in a reply


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious

Messages In This Thread
City Supervisors Meeting - eaadams - 08-31-2011, 12:25 PM
RE: City Supervisors Meeting - rthompson - 08-31-2011, 01:20 PM
RE: City Supervisors Meeting - eaadams - 08-31-2011, 01:35 PM
RE: City Supervisors Meeting - rthompson - 08-31-2011, 11:47 PM
RE: City Supervisors Meeting - eaadams - 09-02-2011, 09:18 AM
RE: City Supervisors Meeting - Ernesto - 09-03-2011, 02:00 PM
RE: City Supervisors Meeting - Ernesto - 09-03-2011, 04:41 PM
RE: City Supervisors Meeting - Ernesto - 09-04-2011, 09:22 AM
RE: City Supervisors Meeting - CC Solutions - 09-04-2011, 10:41 AM