50% fail rate
09-13-2011, 05:44 PM,
#8
RE: 50% fail rate
If one area is high we retest. If it continues to be high, we have a problem in that area and yes we mitigate.
We use reason of course. If the entire slab is at 73% and one area is 76%, well don't tell anyone, but I'll say put the dang floor down. We are pretty dang comfortable with the safety of 80% and under. Now when you start getting to mid 80's I get worried. Do you want a lifetime floor or a one year floor?
Remember I am working with rubber floors and sheet vinyl....
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Quote this message in a reply


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious

Messages In This Thread
50% fail rate - eaadams - 05-27-2011, 10:55 AM
RE: 50% fail rate - EWagner - 05-27-2011, 03:55 PM
RE: 50% fail rate - eaadams - 05-27-2011, 04:57 PM
RE: 50% fail rate - CC Solutions - 05-30-2011, 11:18 AM
RE: 50% fail rate - eaadams - 05-30-2011, 01:24 PM
RE: 50% fail rate - CC Solutions - 09-12-2011, 05:43 PM
RE: 50% fail rate - eaadams - 09-13-2011, 03:07 PM
RE: 50% fail rate - CC Solutions - 09-13-2011, 05:44 PM
RE: 50% fail rate - eaadams - 09-13-2011, 05:50 PM
RE: 50% fail rate - CC Solutions - 09-13-2011, 05:58 PM
RE: 50% fail rate - eaadams - 09-13-2011, 06:01 PM
RE: 50% fail rate - CC Solutions - 09-13-2011, 06:04 PM