This thread is in regards to who is doing the testing of a concrete slab, their qualifications, and their relationship with the parties involved.
IF you choose to test a slab yourself please have a member of your company certified as a flooring inspector. This shows that the individual doing the testing has been trained in the current processes and should know what he is doing.
Hiring an Independent Inspection Firm will free you from liability issues should the concern of biased or unreliable test results arise.
At the very least make sure at least one of your crew has been trained by a recognised certification org and their certs are up to date.
If thats not an option there are many flooring inspectors looking for work right now.
I am a member of these two boards but cannot endorse them.
I can however recommend the individuals listed as the highest qualified flooring inspectors you will find anywhere in the USA.
NICFI - http://www.nicfi.org/
FCITS -www.fcits.org
Another good place to look for certified inspectors is: http://www.floorreports.com

I am not posting this msg to promote any of these sites but offering info to those in need of independent inspection services in their area.
Reply


Messages In This Thread
Certified Testing Results - Wesley Holley - 10-30-2008, 10:52 PM
RE: Certified Testing Results - Ernesto - 09-21-2009, 04:20 PM
RE: Certified Testing Results - fyifloors - 08-11-2010, 12:58 AM
RE: Certified Testing Results - Ernesto - 08-22-2010, 09:44 PM
RE: Certified Testing Results - fyifloors - 08-22-2010, 09:52 PM
RE: Certified Testing Results - Ernesto - 08-23-2010, 08:47 AM
RE: Certified Testing Results - fyifloors - 08-23-2010, 01:48 PM
RE: Certified Testing Results - Ernesto - 08-23-2010, 04:52 PM
RE: Certified Testing Results - fyifloors - 08-24-2010, 04:27 PM
RE: Certified Testing Results - Ernesto - 08-25-2010, 05:03 PM
RE: Certified Testing Results - eaadams - 08-30-2010, 09:53 AM

Possibly Related Threads...
Thread Author Replies Views Last Post
  ICRI pH testing Concrete Repair Bulletin eaadams 4 2,420 05-20-2014, 12:00 PM
Last Post: Ashok Kakade
  Tandus removes moisture testing requirement eaadams 2 4,097 09-27-2013, 10:26 AM
Last Post: eaadams
  RH Testing Thick Slabs CCR 33 48,033 11-21-2012, 10:19 AM
Last Post: eaadams
  Calcium Carbide testing and Silicates Lepito 51 83,172 11-19-2012, 11:59 AM
Last Post: ILLENTINC
  Carbide moisture testing CC Solutions 4 8,677 09-18-2012, 06:11 PM
Last Post: CC Solutions
  Testing Cost eaadams 22 33,539 07-30-2012, 07:01 PM
Last Post: Ernesto
  Questioning the results of RH probes brian 4 9,784 10-13-2011, 03:09 PM
Last Post: CC Solutions
  Another tester brought in to dispute test results. CC Solutions 4 9,705 08-14-2011, 09:32 PM
Last Post: CC Solutions
  Mositure Testing Over Concrete Discussion Ernesto 36 67,859 04-19-2011, 04:59 PM
Last Post: CC Solutions
  I offered free RH testing CC Solutions 9 20,465 04-05-2011, 05:33 AM
Last Post: CC Solutions

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)