Wagner doesn't pay me! In fact I didn't recommend the Rapid Rh, even though it is the most accurate and easy to use RH measuring device on the market! Tongue

I feel comfortable doing both, but I don't put much stock in a MVER reading for the dozens of reasons I have espoused again and again.

If the MVER is at 2lbs and the RH is at 99% what will you do?

Alternately if the RH is at 72% and the MVER is at 6lbs what will you do?
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply


Messages In This Thread
RE: Mositure Testing Over Concrete Discussion - CC Solutions - 04-18-2011, 05:18 PM

Possibly Related Threads...
Thread Author Replies Views Last Post
  ICRI pH testing Concrete Repair Bulletin eaadams 4 2,361 05-20-2014, 12:00 PM
Last Post: Ashok Kakade
  35-40 year old concrete with moisture problems Tscdad 13 7,180 05-19-2014, 10:55 AM
Last Post: eaadams
  Concrete Hood Method Blake McFee 9 27,177 11-08-2013, 01:41 PM
Last Post: eaadams
  Tandus removes moisture testing requirement eaadams 2 4,044 09-27-2013, 10:26 AM
Last Post: eaadams
  RH in Concrete for Wood Floor with Vapor Membrane eaadams 35 63,603 05-01-2013, 07:20 AM
Last Post: jim decker
Question Concrete Cork Sandwich Floor System JKJeremy 4 8,181 01-30-2013, 04:43 PM
Last Post: eaadams
  RH Testing Thick Slabs CCR 33 47,760 11-21-2012, 10:19 AM
Last Post: eaadams
  Calcium Carbide testing and Silicates Lepito 51 82,735 11-19-2012, 11:59 AM
Last Post: ILLENTINC
  Carbide moisture testing CC Solutions 4 8,612 09-18-2012, 06:11 PM
Last Post: CC Solutions
  Testing Cost eaadams 22 33,273 07-30-2012, 07:01 PM
Last Post: Ernesto

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)