Quote:For my own edification: Lets say you have slab on vapor retarder. Slab curls. You grind off the top and lay flooring. The bottom of the curled slab is now plenum space? Can H2O travel laterally in that space?

--------------------------------------------------------------------------------

Can I try and answer that? The vesicular structure in the concrete inhibits the lateral movement of moisture in the slab. But after it moves off the top of the slab it can go anywhere.






Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Reply


Messages In This Thread
RH Numbers Rising - COD - 04-05-2011, 09:40 AM
RE: RH Numbers Rising - eaadams - 04-05-2011, 10:49 AM
RE: RH Numbers Rising - Ernesto - 04-05-2011, 11:49 AM
RE: RH Numbers Rising - eaadams - 04-05-2011, 12:19 PM
RE: RH Numbers Rising - Ernesto - 04-05-2011, 12:27 PM
RE: RH Numbers Rising - COD - 04-05-2011, 01:16 PM
RE: RH Numbers Rising - CC Solutions - 04-05-2011, 05:26 PM
RE: RH Numbers Rising - Ernesto - 04-05-2011, 08:42 PM
RE: RH Numbers Rising - CC Solutions - 04-06-2011, 06:04 AM
RE: RH Numbers Rising - Ernesto - 04-06-2011, 07:40 AM
RE: RH Numbers Rising - CC Solutions - 04-06-2011, 07:47 AM
RE: RH Numbers Rising - Ernesto - 04-06-2011, 08:23 AM
RE: RH Numbers Rising - CC Solutions - 04-06-2011, 08:28 AM
RE: RH Numbers Rising - Ernesto - 04-06-2011, 04:54 PM
RE: RH Numbers Rising - CC Solutions - 04-07-2011, 06:12 AM
RE: RH Numbers Rising - rthompson - 04-07-2011, 01:08 PM
RE: RH Numbers Rising - Ernesto - 04-08-2011, 08:01 AM
RE: RH Numbers Rising - CC Solutions - 04-08-2011, 08:06 AM
RE: RH Numbers Rising - rthompson - 04-08-2011, 10:33 AM
RE: RH Numbers Rising - eaadams - 04-08-2011, 04:19 PM
RE: RH Numbers Rising - Ernesto - 04-08-2011, 04:54 PM
RE: RH Numbers Rising - eaadams - 04-08-2011, 05:00 PM
RE: RH Numbers Rising - CC Solutions - 04-09-2011, 08:59 AM
RE: RH Numbers Rising - rthompson - 04-09-2011, 11:57 AM
RE: RH Numbers Rising - CC Solutions - 04-09-2011, 01:14 PM
RE: RH Numbers Rising - eaadams - 04-09-2011, 01:38 PM
RE: RH Numbers Rising - CC Solutions - 04-09-2011, 01:46 PM
RE: RH Numbers Rising - rthompson - 04-09-2011, 02:06 PM
RE: RH Numbers Rising - CC Solutions - 04-09-2011, 02:39 PM
RE: RH Numbers Rising - Ernesto - 04-11-2011, 09:49 AM
RE: RH Numbers Rising - CC Solutions - 04-11-2011, 09:54 AM
RE: RH Numbers Rising - Ernesto - 04-11-2011, 08:50 PM
RE: RH Numbers Rising - T_Schneider - 04-18-2011, 12:26 PM
RE: RH Numbers Rising - CC Solutions - 04-18-2011, 01:10 PM
RE: RH Numbers Rising - T_Schneider - 04-18-2011, 01:20 PM
RE: RH Numbers Rising - CC Solutions - 04-18-2011, 01:28 PM
RE: RH Numbers Rising - Ernesto - 04-18-2011, 03:08 PM
RE: RH Numbers Rising - eaadams - 04-18-2011, 04:46 PM
RE: RH Numbers Rising - Ernesto - 04-18-2011, 04:55 PM
RE: RH Numbers Rising - CC Solutions - 04-18-2011, 05:15 PM
RE: RH Numbers Rising - Ernesto - 04-20-2011, 07:58 AM
RE: RH Numbers Rising - CC Solutions - 04-20-2011, 08:02 AM
RE: RH Numbers Rising - rthompson - 04-20-2011, 05:15 PM
RE: RH Numbers Rising - CC Solutions - 04-20-2011, 09:00 PM
RE: RH Numbers Rising - Ernesto - 04-23-2011, 07:01 PM
RE: RH Numbers Rising - rthompson - 04-23-2011, 07:59 PM
RE: RH Numbers Rising - CC Solutions - 04-23-2011, 08:59 PM
RE: RH Numbers Rising - rthompson - 04-23-2011, 10:01 PM
RE: RH Numbers Rising - Ernesto - 04-24-2011, 08:24 AM
RE: RH Numbers Rising - eaadams - 09-08-2011, 06:08 PM
RE: RH Numbers Rising - CC Solutions - 09-09-2011, 08:11 AM
RE: RH Numbers Rising - rthompson - 09-09-2011, 09:36 AM
RE: RH Numbers Rising - Ernesto - 09-09-2011, 04:48 PM
RE: RH Numbers Rising - CC Solutions - 09-10-2011, 07:47 AM
RE: RH Numbers Rising - Ernesto - 09-10-2011, 11:14 AM
RE: RH Numbers Rising - CC Solutions - 09-10-2011, 06:30 PM
RE: RH Numbers Rising - Ernesto - 09-11-2011, 08:22 AM
RE: RH Numbers Rising - rthompson - 09-11-2011, 08:25 AM
RE: RH Numbers Rising - Ernesto - 09-11-2011, 08:40 AM
RE: RH Numbers Rising - CC Solutions - 09-11-2011, 03:54 PM
RE: RH Numbers Rising - Ernesto - 09-11-2011, 06:50 PM
RE: RH Numbers Rising - rthompson - 09-12-2011, 08:56 AM
RE: RH Numbers Rising - CC Solutions - 09-12-2011, 09:07 AM
RE: RH Numbers Rising - Ernesto - 09-12-2011, 05:14 PM
RE: RH Numbers Rising - CC Solutions - 09-12-2011, 05:33 PM
RE: RH Numbers Rising - Ernesto - 09-12-2011, 07:27 PM
RE: RH Numbers Rising - CC Solutions - 09-13-2011, 05:52 AM
RE: RH Numbers Rising - Ernesto - 09-13-2011, 07:49 AM
RE: RH Numbers Rising - rthompson - 09-13-2011, 08:37 AM
RE: RH Numbers Rising - CC Solutions - 09-13-2011, 08:43 AM
RE: RH Numbers Rising - Ernesto - 09-13-2011, 10:08 AM
RE: RH Numbers Rising - CC Solutions - 09-13-2011, 11:28 AM
RE: RH Numbers Rising - Ernesto - 09-13-2011, 01:37 PM
RE: RH Numbers Rising - CC Solutions - 09-13-2011, 01:55 PM
RE: RH Numbers Rising - eaadams - 09-13-2011, 02:14 PM
RE: RH Numbers Rising - Ernesto - 09-13-2011, 02:17 PM
RE: RH Numbers Rising - eaadams - 09-13-2011, 02:18 PM
RE: RH Numbers Rising - CC Solutions - 09-13-2011, 02:33 PM
RE: RH Numbers Rising - Ernesto - 09-13-2011, 05:26 PM
RE: RH Numbers Rising - eaadams - 09-13-2011, 05:46 PM
RE: RH Numbers Rising - CC Solutions - 09-13-2011, 05:52 PM
RE: RH Numbers Rising - eaadams - 09-13-2011, 05:56 PM
RE: RH Numbers Rising - CC Solutions - 09-13-2011, 06:03 PM
RE: RH Numbers Rising - eaadams - 09-13-2011, 06:06 PM
RE: RH Numbers Rising - Ernesto - 09-13-2011, 07:23 PM
RE: RH Numbers Rising - Ernesto - 09-14-2011, 06:29 AM
RE: RH Numbers Rising - CC Solutions - 09-14-2011, 06:54 AM
RE: RH Numbers Rising - Ernesto - 09-14-2011, 07:39 PM
RE: RH Numbers Rising - CC Solutions - 09-15-2011, 04:59 AM
RE: RH Numbers Rising - Ernesto - 09-20-2011, 08:07 PM
RE: RH Numbers Rising - CC Solutions - 09-20-2011, 08:30 PM
RE: RH Numbers Rising - Ernesto - 09-21-2011, 08:19 PM
RE: RH Numbers Rising - CC Solutions - 09-21-2011, 09:18 PM
RE: RH Numbers Rising - eaadams - 09-22-2011, 08:39 AM
RE: RH Numbers Rising - CC Solutions - 09-22-2011, 09:28 AM
RE: RH Numbers Rising - Ernesto - 09-22-2011, 07:14 PM
RE: RH Numbers Rising - eaadams - 09-22-2011, 07:50 PM
RE: RH Numbers Rising - Ernesto - 09-22-2011, 08:00 PM
RE: RH Numbers Rising - eaadams - 09-22-2011, 08:48 PM
RE: RH Numbers Rising - CC Solutions - 09-23-2011, 05:54 AM
RE: RH Numbers Rising - Ernesto - 09-23-2011, 06:58 AM
RE: RH Numbers Rising - CC Solutions - 09-23-2011, 10:37 AM

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)