Concrete floor and laminate

#11
Well in my humble opinion the tests performed were near what you would expect after the slab being covered by a nonporous covering like a sheet vinyl. The moisture in the slab equillibrated, moved up to the top like it naturally does. Course those guys who tested your slab probably didn't use the Wagner probes did they?

Anyway, those box store people don't know didily about how to control moisture issues. Out here they have a measure guy carry a concrete moisture meter around. If it reads high they usually walk away. I have never heard of them actually doing a real moisture test. And the managers typically are new business grads and have no flooring experience, met quite a few of them.

I suggest you use this product from Durabond, part of Bostik inc.

http://www.bostik-us.com/files/tdsfiles/d261.pdf

Then use six mil over it, float the floor with the appropriate cushion. Of course the slab needs to be checked for sealers and all that stuff they require. Go to a real flooring store or find a independant contractor who is knowledgeable in these situations.

Option #2, buy a wood like porcelain tile planks



Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Reply


Messages In This Thread
Concrete floor and laminate - morrisey - 03-21-2011, 08:03 AM
RE: Concrete floor and laminate - Ernesto - 03-22-2011, 08:13 AM

Possibly Related Threads...
Thread Author Replies Views Last Post
  ICRI pH testing Concrete Repair Bulletin eaadams 4 2,403 05-20-2014, 12:00 PM
Last Post: Ashok Kakade
  35-40 year old concrete with moisture problems Tscdad 13 7,331 05-19-2014, 10:55 AM
Last Post: eaadams
  Concrete Hood Method Blake McFee 9 27,266 11-08-2013, 01:41 PM
Last Post: eaadams
  How thick is your floor? CC Solutions 21 45,383 07-19-2013, 05:14 PM
Last Post: CCR
  RH in Concrete for Wood Floor with Vapor Membrane eaadams 35 63,889 05-01-2013, 07:20 AM
Last Post: jim decker
Question Concrete Cork Sandwich Floor System JKJeremy 4 8,218 01-30-2013, 04:43 PM
Last Post: eaadams
  Self consolidating concrete (SCC) eaadams 32 60,340 05-08-2012, 07:04 AM
Last Post: CC Solutions
  World of Concrete 2012 eaadams 0 3,427 03-23-2012, 09:40 AM
Last Post: eaadams
  Floor Covering Installer eaadams 2 7,712 12-23-2011, 12:06 PM
Last Post: eaadams
  Old concrete slab moisture DeanC 23 50,546 12-15-2011, 01:20 AM
Last Post: foxgeorge

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)