Ceramic Tile Moisture Problems

#1
Are there any different or unique moisture problems that could occur when installing ceramic tile over concrete as opposed to other products over concrete?
Reply

#2
Yes there are. Although tile is most forgiving about excessive moisture issues it has it's own unique problems. One I can think of off the top of my big head is on large format tile, the thinset will not set. It takes an extra long time to fully cure anyway due to the extra area under the tiles and for that setting compound to dry. Another is efflorescence in the grout. In severe situations discoloration of the tiles can happen, even in porcelain.
Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Reply

#3
Thanks!
Reply


Possibly Related Threads...
Thread Author Replies Views Last Post
  Moisture going up Rubensgt40 3 1,593 07-05-2014, 03:18 AM
Last Post: Rubensgt40
  35-40 year old concrete with moisture problems Tscdad 13 7,454 05-19-2014, 10:55 AM
Last Post: eaadams
  Digital moisture meter QC worker 2 1,889 05-10-2014, 08:07 PM
Last Post: Rubensgt40
  Tandus removes moisture testing requirement eaadams 2 4,119 09-27-2013, 10:26 AM
Last Post: eaadams
  Carbide moisture testing CC Solutions 4 8,693 09-18-2012, 06:11 PM
Last Post: CC Solutions
  Old concrete slab moisture DeanC 23 50,631 12-15-2011, 01:20 AM
Last Post: foxgeorge
  Flooring Manufacturer Warrenty in Relation to Moisture mwoody 5 10,938 08-14-2011, 08:43 PM
Last Post: Ernesto
Sad Is there a way to measure moisture plus cold temperatures sort of like a heat index b Ronald Edberg 4 10,746 07-01-2011, 07:11 PM
Last Post: rthompson
  Concrete Moisture Control Systems BuilderPDX 8 16,872 06-09-2011, 06:09 AM
Last Post: CC Solutions
  The Moisture Webinar Ernesto 17 33,342 04-01-2011, 09:02 PM
Last Post: CC Solutions

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)