Hey guys - it seems like the consensus on this forum is that the Rapid RH is the best way to go for measuring moisture in concrete. Are there any tips and tricks or do's and don'ts that I need to be aware of?
Reply

#2
There's a consensus throughout the industry that the Rapid RH is the best!!! Big Grin

Just follow the directions included in the kit and follow ASTM F2170 and you will be fine.

Tips:

Clean the hole out well, then clean it some more!!!
Don't wobble with the drill! Make a straight 3/4" hole.
Drill to proper depth!
Don't allow debris into the sensor or the hole, keep water out.
The first reading after an hour or so is quite accurate, but for something you can take to the bank, wait 72 hours. (After 4 hours you will be really close, but this is off the record!)
Here's a debated one.... Maybe a mod can jump in if I am wrong....
When measuring concrete poured in a fluted pan, take the thickness of the concrete above the flutes (i.e. 4") and add 1/2 of the depth of the flutes (2" fluted pan means you would add 1" to the 4" for a total of 5") and drill your hole 40% of that measurement. I have not seen official documentation on this issue released yet, so please check beforehand. I believe the new ASTM will address this.

JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply

#3
Get one of the cases to carry them in and or keep them in the house in normal temperatures. Never leave them in a vehicle.
Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Reply

#4
Good point. I bring mine in when staying in a hotel just so they are not subjected to -20 and 120F swings....
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply


Possibly Related Threads...
Thread Author Replies Views Last Post
  Rapid RH 4.0 EX back compatible? Rubensgt40 7 4,205 02-20-2014, 01:49 PM
Last Post: rapidrhrep
  Rapid RH Carrying Case Survives Fire EWagner 1 3,584 04-29-2013, 06:50 PM
Last Post: CC Solutions
  Rapid RH probe out of calibration? Rubensgt40 8 17,422 07-30-2012, 04:42 PM
Last Post: CC Solutions
  WAGNER READERS tbrown 2 8,839 09-20-2010, 02:15 PM
Last Post: CC Solutions

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)