#1
what is difference beween the old reader and the new 4.reader? is one better than the other
Reply

#2
It's longer, initiates the read on contact without the PITA tiny button and stays on longer even after pulling it from the hole.
Reply

#3
I love my Wagners, but now I have to buy new readers.... I'm out of probes and they don't sell the old style, so time to bite the bullet.

The new readers are nice!!!Big Grin