Old Slab Test

#1
Could someone point me to the right way to measure a pre WWII slab that has no moisture membrane under it?
Reply

#2
Like any other slab. However you do need to relate that the test is good for only a few days to weeks depending on weather, rain etc.

IMHO a slab with a vapor barrier under it should not be influenced as much if at all if it's done correctly.
Reply

#3
Sad 
The point is there is no vapor barier.

What environmental conditions will provide the highest reading? a low rh day or a high one?
Reply

#4
Hello eaadams,
What are you looking to do with this slab? If you are just looking to test it then you should test it and report the readings at the time of the test.

If however you are looking to determine the long-term suitability of installing a moisture sensitive flooring, I suggest you refer to ACI-710 which requires a moisture barrier under every slab intended to receive flooring. And all manufacturers will follow ACI 710.

No vapor retarder = unlimited failure potential.
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply

#5
Yes we are putting a vapor sensitive floor covering down. I am awaiting instructions from the national tech manager of the product.
Reply

#6
As my little friend in Phoenix say's "seal it and forget it". Rolleyes
Reply


Possibly Related Threads...
Thread Author Replies Views Last Post
  Burnished vs Floated Slab (Stego) eaadams 4 2,006 05-05-2014, 04:17 PM
Last Post: Ernesto
  measurement in a cold slab Noweare 16 25,130 04-15-2014, 02:30 PM
Last Post: Ernesto
  Test Before You Spec! CCR 6 8,425 05-13-2013, 04:51 PM
Last Post: Ernesto
  slab warmer than air eaadams 1 4,194 01-24-2013, 07:03 PM
Last Post: Rubensgt40
  Cal Chlor Test CCR 10 15,490 01-18-2013, 04:48 PM
Last Post: eaadams
  Old concrete slab moisture DeanC 23 50,549 12-15-2011, 01:20 AM
Last Post: foxgeorge
  **EXPERT Advice Needed** - VERY Moist Slab With LOTS of Vapor! What to do? tileguy555 34 61,182 11-29-2011, 01:18 PM
Last Post: john macdonald
  Another tester brought in to dispute test results. CC Solutions 4 9,699 08-14-2011, 09:32 PM
Last Post: CC Solutions
  Interesting Test Result eaadams 16 30,058 08-08-2011, 11:41 AM
Last Post: CC Solutions
  CONCRETE SLAB THICKNESS MINUS 2 9,747 09-20-2010, 02:25 PM
Last Post: CC Solutions

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)