pH test

#1
I notice that wagner sells pH test with distilled water. I thought it was important to use deionized water? As distilled can still carry a charge that can throw off a pH test.
Reply

#2
From ASTM F710:
5.3.1 To test for pH at the surface of a concrete slab, use wide range pH paper, its associated pH chart, and distilled or deionized water. Place several drops of water on a clean surface of concrete, forming a puddle approximately 1 in. (25 mm) in diameter.

From Wagner:
Both de-ionization and distillation processes remove ions from the water and produce "pure water". De-ionization processes can leave bacteria in water. Distillation leaves pure water. In terms of quality, distilled water is better. The standard calls for using either.

Hope this helps you, eaadams.
-admin
Reply

#3
thank you!
Reply


Possibly Related Threads...
Thread Author Replies Views Last Post
  Test Before You Spec! CCR 6 8,434 05-13-2013, 04:51 PM
Last Post: Ernesto
  Cal Chlor Test CCR 10 15,509 01-18-2013, 04:48 PM
Last Post: eaadams
  Another tester brought in to dispute test results. CC Solutions 4 9,705 08-14-2011, 09:32 PM
Last Post: CC Solutions
  Interesting Test Result eaadams 16 30,072 08-08-2011, 11:41 AM
Last Post: CC Solutions
  How to test RH levels after moisture barrier is used DShenk 3 10,637 08-30-2010, 12:42 PM
Last Post: Ernesto
  Old Slab Test eaadams 5 12,181 07-12-2010, 07:00 PM
Last Post: Ernesto
  Test time for RH test jigar0896 14 31,426 01-15-2010, 09:36 PM
Last Post: CC Solutions
  When to Test CFI 2 8,658 12-16-2009, 11:45 AM
Last Post: CC Solutions
  RH Test Hole Callout Ben 3 11,298 11-04-2008, 10:03 AM
Last Post: rthompson

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)