I think I know the answer - but will run it past my favourite group of online moisture geeks and gurus to create a teachable moment.

A big commercial site, not fully closed yet: Re-readings done a few weeks after initial sensor insertions showed some readings actually higher than the first readings, by up to 3%.

2 x brand new sensors were put into an area approximately 100m2, the area was sealed off with plastic sheets and dehums run for a week. Three weeks after the first readings; one sensor read the same and one was higher by 2.5%.

The surface was highly burnished and a basic bead test didn't penetrate after 60 secs.

Also, the sensor which read higher was in a beam area, but it's unknown exactly how deep the beam is (throughout the site some are 400mm some are 600, all drying from both sides). If it's 600, then I definitely don't have 20% depth, it will be approximately 12% depth. Could this make for fluctuating readings?

Either way, I'm suspecting the burnished surface is seriously preventing the slab from drying.

Thoughts?
The problem with socialism is that you soon run out of other people's money.
- Margaret Thatcher

Reply

#2
is it enclosed & acclimated? That could explain a 2.5% variance.

Big jobs often have doors not on etc... also I just had a project that was getting sun on a probe, that F'd all the readings from that probe.
Reply

#3
Just finished an engineered glue down job where an additional ten feet of concrete was added on. New slab was slightly reflective and burnished, so I scarified it with my grinder a bit. It dropped 5 points in two weeks.
I profile all my slabs anyways so the glue sticks better, gets rid of any contaminants yata yata yata.
Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Reply

#4
Thanks everyone. It's probably all of the above. Very open site, and the slab is just too burnished. Did some more readings last week and they've hardly moved.
The problem with socialism is that you soon run out of other people's money.
- Margaret Thatcher

Reply


Possibly Related Threads...
Thread Author Replies Views Last Post
  35-40 year old concrete with moisture problems Tscdad 13 7,412 05-19-2014, 10:55 AM
Last Post: eaadams
  Digital moisture meter QC worker 2 1,889 05-10-2014, 08:07 PM
Last Post: Rubensgt40
  Tandus removes moisture testing requirement eaadams 2 4,118 09-27-2013, 10:26 AM
Last Post: eaadams
  Carbide moisture testing CC Solutions 4 8,692 09-18-2012, 06:11 PM
Last Post: CC Solutions
  Old concrete slab moisture DeanC 23 50,609 12-15-2011, 01:20 AM
Last Post: foxgeorge
  Flooring Manufacturer Warrenty in Relation to Moisture mwoody 5 10,935 08-14-2011, 08:43 PM
Last Post: Ernesto
Sad Is there a way to measure moisture plus cold temperatures sort of like a heat index b Ronald Edberg 4 10,745 07-01-2011, 07:11 PM
Last Post: rthompson
  Concrete Moisture Control Systems BuilderPDX 8 16,865 06-09-2011, 06:09 AM
Last Post: CC Solutions
  The Moisture Webinar Ernesto 17 33,334 04-01-2011, 09:02 PM
Last Post: CC Solutions
  Ceramic Tile Moisture Problems DeanC 2 9,096 03-07-2011, 03:47 PM
Last Post: DeanC

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)