Rapid RH 4.0 EX back compatible?

#1
I wonder if that shadowy, mysterious chap who goes deep cover under the name of "rapidrhrep" might weigh in on this:

I got the exchange reader today with a batch of new 4.0 EX probes.

So what's the diff? I note that the new reader still seems to read the old probes. I've had some "re-read" requests lately so this is a relief.

Also, what about the bluetooth datamaster reader- does it read the new probes?
The problem with socialism is that you soon run out of other people's money.
- Margaret Thatcher

Reply

#2
Wow, I figured after hearing about your summer "down under", you would have melted away by now. The answer to your question revolves around technology and an upgrade to the readers "software". Nothing that anybody would ever notice with regards to performance of the product in the field. Regarding the Datamaster, it is forward and backwards compatible. Thanks for the comment and sorry for the delay.

Jason
Reply

#3
Thanks Mr. Rep.

Re our summer- nothing we can't handle Big Grin I think your midwestern coldsnap would be a trickier thing!

Although I did send you a PM re some other issues, if you could follow up that would be grouse. (That's Oz-strayan for great)
The problem with socialism is that you soon run out of other people's money.
- Margaret Thatcher

Reply

#4
(02-03-2014, 09:52 PM)Rubensgt40 Wrote:  Thanks Mr. Rep.

Re our summer- nothing we can't handle Big Grin I think your midwestern coldsnap would be a trickier thing!

We have the same weather here in southern Arizona. Not a problem here either. Cool
Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Reply

#5
I was told that the old reader will read new EX probes as 99% but the new reader will read new and old probes fine.
Reply

#6
The "old" reader will produce an "Er" reading on the EX sensors. The "new" reader will read both just fine.

Jason
Reply

#7
thanks for posting that. was about to say something incorrect to a a GC.
Reply

#8
I got yer back EA!
Reply


Possibly Related Threads...
Thread Author Replies Views Last Post
  Rapid RH Carrying Case Survives Fire EWagner 1 3,543 04-29-2013, 06:50 PM
Last Post: CC Solutions
  Rapid RH probe out of calibration? Rubensgt40 8 17,311 07-30-2012, 04:42 PM
Last Post: CC Solutions
  Do's and Don'ts for the Wagner Rapid RH DeanC 3 10,844 02-21-2011, 02:50 PM
Last Post: CC Solutions

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)