How to test RH levels after moisture barrier is used

#1
Here is my situation: Tested the conc with an RH level of 90%, using Bamboo floor covering that requires a moisture barrier. After installing the moisture barrier how do I determine if the moisture levels have reduced to the acceptable levels to install the bamboo? Do I use a CaCl test since I am now just concerned with the surface reading?
Thanks.
Reply

#2
I think the two preferred methods will be the CaCl test ASTM F1869 and the RH Hood test ASTM F2420.

Personally I would use the CaCl test because that is probably what the flooring manufacturer is looking for. In this case the MVER will not vary much because of the mitigation system in place.

This test should be conducted directly on the moisture barrier, not over any patch material.
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply

#3
(01-21-2010, 02:30 PM)DShenk Wrote:  the moisture barrier

Is it a moisture barrier (VAP, Planiseal, MC) or is it a vapor membrane (visquene 6mil from Home Despot) or is a low perm vapor barrier (Stego, Reef or equal) ?
Reply

#4
Is it gluedown? Bamboo over a slab reading 90% Thats one I would not feel bad about walking away from.
Reply


Possibly Related Threads...
Thread Author Replies Views Last Post
  Moisture going up Rubensgt40 3 1,550 07-05-2014, 03:18 AM
Last Post: Rubensgt40
  35-40 year old concrete with moisture problems Tscdad 13 7,346 05-19-2014, 10:55 AM
Last Post: eaadams
  Digital moisture meter QC worker 2 1,855 05-10-2014, 08:07 PM
Last Post: Rubensgt40
  Tandus removes moisture testing requirement eaadams 2 4,088 09-27-2013, 10:26 AM
Last Post: eaadams
  Test Before You Spec! CCR 6 8,426 05-13-2013, 04:51 PM
Last Post: Ernesto
  Cal Chlor Test CCR 10 15,498 01-18-2013, 04:48 PM
Last Post: eaadams
  Carbide moisture testing CC Solutions 4 8,672 09-18-2012, 06:11 PM
Last Post: CC Solutions
  Old concrete slab moisture DeanC 23 50,563 12-15-2011, 01:20 AM
Last Post: foxgeorge
  Another tester brought in to dispute test results. CC Solutions 4 9,700 08-14-2011, 09:32 PM
Last Post: CC Solutions
  Flooring Manufacturer Warrenty in Relation to Moisture mwoody 5 10,918 08-14-2011, 08:43 PM
Last Post: Ernesto

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)