Tested a slab on grade, almost in the wash, probably one of the lowest points in the area as far as water tables run. Got readings of 67 to 70% rh @ 70 to 72 F. Getting tons of rain down here and water puddles in the yard. Home is 15 years old at least so doubt there is a vapor barrier underneath. I was certain I would get at least a 95% rh. Goes to show you never know. I be gluing some engineered hardwood down with Sika T-21.

Didja know Sika has no numbers for either 1869 or 2170?
Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Reply

#2
I've seen a number of manufacturers of various products who don't state tolerance levels or requirements. Surprising to say the least.
JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com
Reply

#3
I had some test results just come back on a project.

Slab is 2.5 years old and I was convinced it would come in wet.

Every test came in from the 70s - 80s. Thoroughly surprised.
Reply

#4
Well that's great!
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply


Possibly Related Threads...
Thread Author Replies Views Last Post
  Ardex promotes the Wagner Rapid RH probe! CC Solutions 15 35,058 01-15-2012, 06:33 PM
Last Post: CC Solutions
  High Rapid RH readings?? ddemento 49 81,042 12-08-2011, 06:03 PM
Last Post: Ernesto
  MMS- Are some unreliable with high RH? Rubensgt40 64 101,773 11-17-2011, 07:56 AM
Last Post: CC Solutions
  No Love - August Rapid RH Newsletter eaadams 4 9,336 08-19-2011, 07:13 AM
Last Post: CC Solutions
  high rh in concrete chas04344 2 8,899 09-11-2009, 07:33 PM
Last Post: chas04344

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)