Can anyone share any experience in performing RH tests in these exterior "unacclimated" environments? Concrete over steel decking precisely.
JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com
Reply

#2
Hopefully your climate is stable and not fluctuating wildly.... Temperature is a factor of rH!
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply

#3
Well, it's Pittsburgh, what can I say except temp at testing time was my first concern too. But this is no place to do Calcium Chloride tests. I would anticipate performing tests in the late spring thru early fall about the same time and ambient conditions the coating systems are to be applied. So technically, they would be conducted in conditions the manufacturer would recognize as acclimated (for application anyway). Other than that, I can think of nothing else to be concerned with off the top of my head.

I'm writing "blindly" right now because I have not read the manufacturer's literature yet. That's next

Always something new to consider, right?
JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com
Reply

#4
I would ask the manufacturer for their requirements first. If the coating is quite breathable they may be rather lax in their demands.

Typically though almost any finish requires some degree of dryness be inherent in the substrate. You wouldn't put ceramic tile on a 2 day old slab, but 30 days may be fine.

Determining the dryness is rather easy if the slab reaches a temperature conducive for testing. If the concrete never falls below 90 degrees, the rH can read quite low, yet the moisture present could be rather high. Likewise in the winter a cold slab would read artificially low. This is why we test at a standard expected temperature. Outside that range is going to be very wide spread, but you may get a good idea of comparable rH if you can read the slab around 70 degrees.

If the temperature is moving quickly, you may need to insure your probe and the sensor are acclimated also. Can you shade the area you are reading?
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply

#5
Appreciate your inputExclamation It appears all their coating systems call for CaCl testing. I can see it now...prep the test area, etc. per ASTM, place the kits and come to find a virtual rain forest inside the plastic cover and pellets solidified into a slimy, solid mass. Big Grin
JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com
Reply

#6
A lot of manufacturers if you call them have unpublished RH limits.
Reply

#7
True. I will definitely inquire on that.

Thanks.
JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com
Reply


Possibly Related Threads...
Thread Author Replies Views Last Post
Wink article on testing eaadams 3 6,308 09-01-2013, 09:10 AM
Last Post: CC Solutions
  No Testing Requirements ???? CCR 3 5,180 06-28-2013, 10:26 AM
Last Post: eaadams
  Moisture Testing Awareness raised Down Under... Horror abounds... Rubensgt40 6 9,612 05-10-2013, 06:46 PM
Last Post: Rubensgt40
  insuti testing jim decker 27 26,993 05-02-2013, 12:31 PM
Last Post: jim decker
  How Do You Charge For Testing? CCR 23 22,681 03-21-2013, 05:05 PM
Last Post: CCR
  RH & CC Testing CCR 23 41,601 07-26-2012, 06:19 AM
Last Post: CC Solutions
  Wood Floor Testing eaadams 1 5,426 06-07-2012, 01:08 PM
Last Post: hnelson

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)