I am going over to Hawaii to install a large marble floor on a concrete slab. This will be a new slab. Is there anything I need to know about moisture in the slab in Hawaii that won't be taken care of with the vapor barrier after a 28 day cure due to the humidity or anything else? This is above grade.
Reply

#2
You’ll get to know Hawaii pretty well if the slab has only had 28 days to cure. You still have to wait for it to dry after its cured. That can take months even if youre in the Mohave desert. If you want it to dry quicker, I’d suggest you get the room enclosed with big fans. Or you can put a sealant on the concrete to keep the moisture from coming up. I'd rather wait around and see Hawaii.
Reply

#3
Thankfully Hawaii is pretty much permanently humid..it's all relative..no pun intended... The dryness is a relative factor and it is actually best if concrete never drop below an internal r.h. of 80% which allows the concrete to continue curing..the longer concrete cures, the denser it becomes, the the relative amount of moisture available in the pores becomes less and less of an issue..the denser the concrete, the smaller the pores and the fewer remain connected...
Reply


Possibly Related Threads...
Thread Author Replies Views Last Post
  Moisture going up Rubensgt40 3 1,600 07-05-2014, 03:18 AM
Last Post: Rubensgt40
  ICRI pH testing Concrete Repair Bulletin eaadams 4 2,480 05-20-2014, 12:00 PM
Last Post: Ashok Kakade
  35-40 year old concrete with moisture problems Tscdad 13 7,475 05-19-2014, 10:55 AM
Last Post: eaadams
  Digital moisture meter QC worker 2 1,904 05-10-2014, 08:07 PM
Last Post: Rubensgt40
  Burnished vs Floated Slab (Stego) eaadams 4 2,057 05-05-2014, 04:17 PM
Last Post: Ernesto
  measurement in a cold slab Noweare 16 25,269 04-15-2014, 02:30 PM
Last Post: Ernesto
  Concrete Hood Method Blake McFee 9 27,376 11-08-2013, 01:41 PM
Last Post: eaadams
  Tandus removes moisture testing requirement eaadams 2 4,132 09-27-2013, 10:26 AM
Last Post: eaadams
  RH in Concrete for Wood Floor with Vapor Membrane eaadams 35 64,208 05-01-2013, 07:20 AM
Last Post: jim decker
Question Concrete Cork Sandwich Floor System JKJeremy 4 8,264 01-30-2013, 04:43 PM
Last Post: eaadams

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)