#1
I have heard that a surface moisture meter is not as good a way to measure moisture in concrete as using an internal relative humidity sensor. Could someone clarify this for me?
Reply

#2
Blake,
Correct, surface moisture meters and surface testing measures the very top of the concrete. As concrete dries from the top down, the slab may be wet at the bottom while indicating dry at the surface. Once a slab is covered with a moisture sensitive flooring the slab will go into equilibrium and the moisture will increase at the surface. The use of a RH Sensor will measure the internal moisture at the apex of the drying curve, which is the point where equilibrium crosses.
Please advise any questions
Rayt
Reply

#3
Thanks, and how deep should I measure to get to the equilibrium point?

Blake
Reply

#4
ASTM F-2170 recommends 40% the thickness of the slab
Rayt
Reply

#5
Blake,
About 40% the thickness of the slab. 4" slab about 1-1/2 - 1-3/4"
Rayt
Reply


Possibly Related Threads...
Thread Author Replies Views Last Post
  Moisture going up Rubensgt40 3 1,543 07-05-2014, 03:18 AM
Last Post: Rubensgt40
  35-40 year old concrete with moisture problems Tscdad 13 7,305 05-19-2014, 10:55 AM
Last Post: eaadams
  Digital moisture meter QC worker 2 1,847 05-10-2014, 08:07 PM
Last Post: Rubensgt40
  Tandus removes moisture testing requirement eaadams 2 4,073 09-27-2013, 10:26 AM
Last Post: eaadams
  Carbide moisture testing CC Solutions 4 8,659 09-18-2012, 06:11 PM
Last Post: CC Solutions
  Old concrete slab moisture DeanC 23 50,519 12-15-2011, 01:20 AM
Last Post: foxgeorge
  Flooring Manufacturer Warrenty in Relation to Moisture mwoody 5 10,908 08-14-2011, 08:43 PM
Last Post: Ernesto
Sad Is there a way to measure moisture plus cold temperatures sort of like a heat index b Ronald Edberg 4 10,714 07-01-2011, 07:11 PM
Last Post: rthompson
  Concrete Moisture Control Systems BuilderPDX 8 16,821 06-09-2011, 06:09 AM
Last Post: CC Solutions
  The Moisture Webinar Ernesto 17 33,266 04-01-2011, 09:02 PM
Last Post: CC Solutions

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)