I just had a proposal come across my desk referancing ASTM E 1907-06a Standard Guide to Methods of Evaluating Moisture Conditions of Concrete Floors to Receive Resilient Floor Coverings.

Can anyone give me some background on it?

I read it was withdrawn and replaced by F710. So.... what should I think?

http://www.astm.org/Standards/E1907.htm
Reply

#2
Yeah, that's an old standard....
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply

#3
Was that an architectural spec? Wouldn't surprise me if it was considering how so many just cut and paste with no clue what they're preparing for bid.Confused
JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com
Reply

#4
It was actually in a proposal from an ICRI testing company. I called them on it. Seems to me it may be trying to over complicate the proposal with ASTM.

But whatever, I gave their proposal to the client along with 3 others.
Reply


Possibly Related Threads...
Thread Author Replies Views Last Post
  astm meeting last week eaadams 5 2,802 05-16-2014, 07:53 AM
Last Post: rhguru
  ASTM F2170 Certification? jpeters 16 37,092 05-04-2010, 02:22 PM
Last Post: budley-19

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)