I've got a deck that I've got to measure, and I hear that they dry differently, or that ASTM classifies them differently, or something along those lines, because it's up off the ground. Is that true?
Reply

#2
Is your concrete slab on a metal deck? How did you pour it?

Basically, ASTM F2170 says that if the slab is drying only from the top, you should drill to 40% into it for your test. If it's drying from both sides (which means it's not on a metal deck or sitting on the ground with a vapor retarder below) than you only should drill down 20% of the thickness
Reply


Possibly Related Threads...
Thread Author Replies Views Last Post
  Not so fast... it is going to take time e.g. RH from 7/25 - 9/5 eaadams 0 412 09-16-2014, 12:19 PM
Last Post: eaadams
  ICRI pH testing Concrete Repair Bulletin eaadams 4 2,412 05-20-2014, 12:00 PM
Last Post: Ashok Kakade
  35-40 year old concrete with moisture problems Tscdad 13 7,350 05-19-2014, 10:55 AM
Last Post: eaadams
  Burnished vs Floated Slab (Stego) eaadams 4 2,009 05-05-2014, 04:17 PM
Last Post: Ernesto
  measurement in a cold slab Noweare 16 25,136 04-15-2014, 02:30 PM
Last Post: Ernesto
  Concrete Hood Method Blake McFee 9 27,282 11-08-2013, 01:41 PM
Last Post: eaadams
  RH in Concrete for Wood Floor with Vapor Membrane eaadams 35 63,936 05-01-2013, 07:20 AM
Last Post: jim decker
Question Concrete Cork Sandwich Floor System JKJeremy 4 8,224 01-30-2013, 04:43 PM
Last Post: eaadams
  slab warmer than air eaadams 1 4,195 01-24-2013, 07:03 PM
Last Post: Rubensgt40
  Self consolidating concrete (SCC) eaadams 32 60,370 05-08-2012, 07:04 AM
Last Post: CC Solutions

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)